Ask what a brass foil expands by and the working answer is 18 to 20 parts per million per degree Celsius. It is a high figure compared with many engineering metals, and it is the root of most failures where brass foil is bonded to something that moves less. Here is how the number is defined, what shifts it, and where it bites in practice.
What exactly does the CTE number mean?
The coefficient of thermal expansion is strain per degree of temperature change. A value of 18 x10^-6 /C means a one-metre length grows by 18 micrometres for each degree it warms. The length change follows a simple relation: ΔL = L0 x α x ΔT, where L0 is the starting length, α the coefficient and ΔT the temperature swing. The arithmetic is easy; the difficulty is that α is not a fixed constant across all brasses.

Brass is copper plus zinc, and the zinc content moves the coefficient. Rolling direction adds a smaller effect, because worked foil is slightly anisotropic - it expands a little differently along the rolling direction than across it. Heat treatment changes it again by altering residual stress. For a design that lives near a CTE limit, specify the alloy and temper, not just the word brass.
Where does a high CTE become a problem?
On a printed circuit board, brass foil used as a conductive path is bonded to a substrate whose expansion is often much lower. Heat the assembly through reflow or service and the two layers want different lengths; the resulting shear shows up as bow, delamination or a cracked joint after repeated cycles. Our high-conductivity RA brass foil is produced with a controlled coefficient so the mismatch stays predictable when it sits against common substrate materials.

Heat exchangers present the opposite case. There a foil that expands more can be an asset - it helps a brazed joint stay in compression - provided the joint design accounts for it. Stamped decorative parts are more forgiving still, since they are usually free to move. The same number is therefore a constraint in one application and a non-issue in another; the deciding factor is what the foil is bonded to.
How should a designer use the figure?
Compute the length change over the full service temperature range, not a nominal room-temperature delta, and compare it with the adjacent material. If the difference is large, either choose an alloy with a closer coefficient - a lower-zinc brass or a rolled brass foil to a different temper - or change the geometry to relieve strain, such as a narrower trace or a compliant bond line. Ask us for the measured coefficient on the specific lot if your tolerance is tight; catalogue values are averages across compositions.
Share your temperature range, the material the foil is bonded to and the allowed dimensional drift, and we will confirm whether the standard grade fits or a different alloy should be quoted.
Is brass CTE higher or lower than copper?
Slightly higher in most brass grades. Copper is around 16 to 17 x10^-6 /C; brass with significant zinc content moves toward 18 to 20.
Does CTE change with foil thickness?
Not materially. The coefficient is a material property; thickness changes the absolute expansion but not the per-degree rate.
Can I get a brass foil with a lower expansion?
Within the brass family the range is limited. If a much lower CTE is required, copper or an invar-type alloy is a more realistic choice. We can discuss the trade-off against conductivity.